Blog

POCO Graphite: Choosing Grades for EDM Electrodes

This guide explains how to read the published data and match grades to the electrode's job.

For most precision sinker work, POCO EDM-3 is the sensible starting grade. Move to EDM-4 or the submicron EDM-AF5 when you need finer detail and finish, use EDM-200 for large and cost conscious electrodes, and reach for a copper infiltrated grade such as EDM-C3 when electrodes are fragile or flushing is poor. Each grade trades particle size, strength, hardness and resistivity differently, and those traits decide electrode wear, surface finish and how many electrodes a job consumes.

A roughing electrode for a forging die and a thin rib finishing electrode for a precision mold need different things from the same block of graphite. Picking the wrong one shows up as extra electrodes, longer burns or ribs that break halfway through. This guide explains how to read the published data and match grades to the electrode's job. POCO is a trademark of Entegris, and all grade values below come from the Entegris POCO EDM grade chart.

Reading a Graphite Datasheet

Four published values do most of the work when choosing an electrode grade.

Particle size. Each spark dislodges tiny pieces of graphite, so smaller particles leave smaller pits. That supports sharper corners, better detail and smoother finishes. Particle size is the most useful single predictor of how a grade will burn.

Flexural strength. This is how much bending load the graphite takes before it breaks. It matters most on thin ribs, tall narrow features and small pins, which have to survive milling, handling, mounting and flushing pressure during the burn.

Hardness. Harder graphite holds edges well but can chip during electrode milling, so it rewards good tooling and toolpaths.

Electrical resistivity. Lower resistivity lets current flow more easily through the electrode. Copper infiltrated grades are far lower than plain graphite, which helps stabilize cutting.

How the POCO EDM Grades Compare

Entegris publishes these typical values for its EDM grades:

  • EDM-200 (Superfine): 10 micron particle size, 9,000 psi flexural strength, 580 microhm-inch resistivity. Good strength, finish and wear for its price.
  • EDM-C200 (Superfine, copper infiltrated): 10 micron, 12,100 psi, Shore 62, 114 microhm-inch. Improves cutting stability where flushing is poor.
  • EDM-1 (Ultrafine): under 5 micron, 9,700 psi, Shore 69, 760 microhm-inch. Good wear, speed and finish at an economical price.
  • EDM-2 (Ultrafine): under 5 micron, 11,200 psi, Shore 71, 620 microhm-inch. Higher strength with good wear resistance.
  • EDM-3 (Ultrafine): under 5 micron, 13,300 psi, Shore 73, 615 microhm-inch. The widely used industry standard precision grade.
  • EDM-C3 (Ultrafine, copper infiltrated): under 5 micron, 20,300 psi, Shore 66, 127 microhm-inch. The strongest grade in the line, suited to fragile electrodes.
  • EDM-4 (Ultrafine): under 4 micron, 17,500 psi, Shore 76, 500 microhm-inch. High strength for intricate electrodes.
  • EDM-AF5 (Angstrofine): under 1 micron, 14,500 psi, Shore 83, 850 microhm-inch. The finest particle size, for extreme detail and fine finishes.

Matching the Grade to the Electrode's Job

Start with what the electrode has to do, then pick the grade.

Roughing electrodes

Roughing calls for fast removal at sensible cost. EDM-200 or EDM-1 can handle bulk removal in large cavities, paired with a premium grade for finishing. Keep an eye on corner wear, because worn roughing corners leave extra stock for the finishing electrode to clean up.

Finishing electrodes

Choose a finishing grade that matches the surface on the drawing. EDM-3 covers a broad range of mold finishes. EDM-4 and EDM-AF5 suit tighter finish and detail requirements, including engraving, micro detail and high polish mold surfaces.

Thin ribs and fine detail

When feature survival is the risk, compare grades by flexural strength first. EDM-C3 and EDM-4 lead the line. A stronger blank costs more, but a rib that breaks mid-burn costs a new electrode, lost machine time and sometimes the cavity.

Good electrode results also depend on how the graphite is cut. Our guide to graphite milling for EDM electrodes covers toolpaths, dust control and edge protection, and our overview of graphite tooling covers holding electrode geometry consistent from blank to burn.

Ribs breaking or finishing electrodes losing detail? Our engineers can look at your electrode design and suggest a grade and tooling for the burn. Talk to an Engineer.

Proving the Grade on Your Own Machine

A datasheet gives a starting point. Your machine shows how a grade performs in practice. Burn settings, workpiece material, flushing and dielectric condition all shift wear and finish in ways a chart cannot predict. A grade that wears well at one on-time can wear faster at another, and steel, carbide and nickel alloys each respond differently.

Run a fair comparison: same electrode shape, same settings, same workpiece material, one variable changed at a time. Record end and corner wear, total burn time, measured finish and any arcing or unstable cutting. A sinker with stable gap control makes these trials meaningful, and EDM Zap's Advantage series power supplies use a proprietary discharge waveform designed to keep electrode wear low, which makes premium grades go further.

Judge grades by cost per part

The graphite blank is a small share of total job cost. Milling time, burn hours, labor and the number of electrodes made all depend on the grade. Count every electrode and every hour of burn time, then compare grades by total cost per finished part rather than price per block.

Ordering Electrode Material

Write the full grade name on the purchase order, such as EDM-3 or EDM-C3, and specify the stock form and a blank size that leaves enough clamping stock for milling. Aerospace and energy customers often need lot traceability, so request certification paperwork up front. Entegris also makes graphite for many non-EDM uses, so make sure the order comes from the EDM grade list.

EDM Zap supplies EDM electrodes and consumables, including graphite, copper and brass electrodes in standard and custom geometries, along with filters, dielectric fluid, fixtures and electrode holders.

Picking a Grade With Confidence

Begin with EDM-3 for general precision work. Step up to EDM-4 or EDM-AF5 for more detail and finer finish, use EDM-200 for large and economical roughers, choose EDM-C3 for fragile features and EDM-C200 where flushing is poor. Then prove your top choice on your own machine and compare by cost per part.

If you are deciding between grades for a tough rib, a fine finish or a large rougher, our team can review your setup and supply the electrodes and tooling to match. Our engineers respond to inquiries within 24 hours. Request a Quote, or call (630) 852 1699.

Frequently Asked Questions

What is POCO graphite used for in EDM?

POCO graphite is used to make sinker EDM electrodes, the shaped tools that burn cavities and forms into the workpiece. Graphite machines easily and handles the heat of the process well.

What is the difference between POCO EDM-3 and EDM-4?

EDM-4 has a smaller particle size and higher strength. EDM-4 is under 4 microns with 17,500 psi flexural strength, while EDM-3 is under 5 microns with 13,300 psi. EDM-3 is the general standard and EDM-4 suits more intricate electrodes.

Does finer graphite always give a better finish?

No. Finer graphite supports a better finish, but power supply settings, flushing and dielectric condition also shape the surface. A fine grade burned at rough settings will still leave a rough surface.

When should I use copper infiltrated graphite?

Use it for fragile electrodes or where flushing is poor. EDM-C3 offers the highest strength in the line for thin features, and EDM-C200 improves cutting stability where debris builds up. Both cost more, so save them for jobs where plain graphite struggles.

Forging

Have an EDM Challenge We Haven't Covered?

Our engineers are happy to answer technical questions directly. Get in touch and we’ll get back to you within 24 hours.

Request a Quote

Thank you! Your submission has been received!
Oops! Something went wrong while submitting the form.